TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Date:
Tue, 28 Jan 2003 08:27:10 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ong Seet Leng <[log in to unmask]>
Subject:
From:
Ong Seet Leng <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
DSO National Laboratories
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
THANKS!

"Dehoyos, Ramon" wrote:

>         Ong:
>         There is a tool that resembles a comb that measures wet thickness.
> One of the companies that carries it is Nordson, a company that manufactures
> CC spraying machines.
>         Good luck, Ramon
>
> > -----Original Message-----
> > From: Ong Seet Leng [SMTP:[log in to unmask]]
> > Sent: Thursday, January 23, 2003 9:51 PM
> > To:   [log in to unmask]
> > Subject:      [TN] ADVISE NEEDED
> >
> > Morning Technetters,
> >
> > Advise needed. We used to use dipped in method using a conformal coating
> > machine but as the latex used to cover the forbidden area need at least a
> > few hours to cure, we cannot afford the time. Due to the extremely tight
> > schedule given to us, we have engineers sending in assembled boards in the
> > morning and expect us to perform miracles and have them ready before
> > lunch.
> >
> > We are now using the hand brush method but as mentioned, due to the
> > extremely tight schedule, is there any way to measure the coating
> > thickness without say, measure assembled board before coat, after that
> > coat one side-measure again, before coat the other side & measure again in
> > order to get the individual side coating thickness?
> >
> > We may have used the wrong approach and I desperately need some advise
> > from you guys and gals. More over, should we revert back to dip in method,
> > how are one going to measure the coating thickness of one side and then
> > protected it before proceed to the un-coated side? Any suggestions is
> > greatly appriciated.
> >
> > Regards
> > S L Ong
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2