TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Date:
Tue, 16 Jul 2002 08:25:49 EDT
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (41 lines)
Hi Terry,
>My thermal stressing uses the following parameters:
>10 cycles of hot / cold exposure in a HALT chamber,
>-60 deg C to +120 deg C temperature excursions,
>40 deg C per minute temperature ramp rate.
>The boards are electrically tested after thermal stressing.
A: The ramp rate surely is not correct. What exactly is a "HALT" chamber?
Depending on the nature of the failures you experience, your testing is not
much of an ESS, and electrically testing after, not during, thermal stressing
will show little even if latent defects are precipitated to failure.
>I calculate the screening is using approximately 20% of the expected life of
the
>assembled boards, so I am reluctant to increase the stress levels.
A: On the basis of what model do you make this calculation? You do nopt even
have a failure mode, let alone a root-cause failure mechanis.
>My board manufacturer has made several process improvements over the last
year but
>I have not seen a significant improvement in my assembly yield.
A: Again. without knowing what is really happening, what the design details
are, and how these PCBs are used, it is impossible to make concrete
recommendations.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2