IPC-4101/40&41 are both polyimide.
I think the only difference is the Tg
40 has a minimum Tg of 200ºC
41 has a minimum Tg of 250ºC
So a 41 would meet the 40 spec.
hope this helps
Geoff Layhe
-----Original Message-----
From: Collins Graham [mailto:[log in to unmask]]
Sent: Thursday, September 25, 2003 5:12 PM
To: [log in to unmask]
Subject: [TN] prepreg classification
Hello Folks!
A question for someone with knowledge of PWB laminant materials. I'm
sure IPC-4101 would tell me, but I don't have it.
If I've ordered material per IPC-4101/40, and have received material
per IPC-4101/41, is the /41 material:
a) the same material but tested to a higher standard?
b) better than but a different material?
c) worse than?
d) some combination of these?
I know the /40 is a polyimide material, I don't know what a /41 is.
Thanks!
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by replying
to it and then delete the message from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|