TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 18 Jan 2006 15:31:39 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard D." <[log in to unmask]>
Parts/Attachments:
text/plain (95 lines)
There are nice examples of the differences in BGA spheres soldered in
nitrogen and air in IPC 7095, if you need documentation to prove your
point. They are shown in section 9.6. 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, January 18, 2006 3:08 PM
To: [log in to unmask]
Subject: Re: [TN] Time to fish or cut bait

You can, but with a higher DPMO. Nitrogen reduces the ability to form
oxides that prevent wetting just prior and during reflow. Without it,
and especially at higher temperatures with alloys that are more
resistant to wetting than 63/37, the difference becomes greater,
especially on BGAs.
The price of the nitrogen option is usually not a great amount. I would
recommend buying it with the capability to do so.
You may need every weapon you can find in your arsenal to promote
wetting to the outer edges of the pads, and being able to get solder to
fully flow over the terminations using the Pb-free alloys.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Neil Maloney
Sent: Wednesday, January 18, 2006 2:32 PM
To: [log in to unmask]
Subject: [TN] Time to fish or cut bait

Greetings, Technet!
 
My company is making the transition from leaded to lead -free assembly
in the US (we have already converted our overseas facility) Now we are
in the throes of the N2 vs. air battle.   Our overseas unit uses air
only without any problems  (ENIG boards, 0602s to QFPs, no BGAs)   In
the US we are looking to start designing  BGA and flip-chip assemblies
with the same type ENIG and Entek boards.  We are buying a new 10 zone
reflow oven, and battle begins. Do we start with nitrogen or not? Can a
small company make lead-free BGA assemblies without going to an N2
atmosphere? 
 
Does air make the process window too small for BGA?
 
Our smallest PCB is about 8x12cm.
 
 
Thanks in advance
     
 
Neil Maloney, Manufacturing Engineer
Contemporary Control Systems, inc
2431 Curtiss St Downers Grove, IL  60515
(630) 963-7070 x132
[log in to unmask]
http://www.ccontrols.com <http://www.ccontrols.com/>
http://www.ctrlink.com <http://www.ctrlink.com/> 
 
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2