Rick,
The IPC spec for ENIG, which is near release, specifies 120-240
microinches of Ni and 2-4 microinches of Au.
Marion Graybeal
----- Original Message -----
From: Rick Thompson <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 30, 2002 7:36 PM
Subject: [TN] ENIG Thickness Standard?
> Is there a standard for the plating thickness of the ENIG surface
> finish? I've searched the archives and didn't find anything. Based on
> a customer request we had increased the requirement for the electroless
> nickel to 200u inches. A couple of our board vendors are telling me that
> that is excessive and that anything over 100u inches is overkill. I've
> seen references in the archives for anything from 120u inches to 200u
> inches. What (if anything) is considered standard for this finish?
>
> Thanks for your inputs.
>
>
> Rick Thompson
> Ventura Electronics Assembly
> 2655 Park Center Dr.
> Simi Valley, CA 93065
>
> +1 (805) 584-9858 x-304 voice
> +1 (805) 584-1529 fax
> [log in to unmask]
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|