At 07:36 AM 4/23/2010, David D. Hillman wrote:
>Hi Guy - oops, sorry about that! BCC stands for Body Centered Cubic
>crystal structure. The metallic elements can be classified in different
>crystal structures: Triclinic, Monoclinic, Orthorhombic, Tetragonal,
>Hexagonal, Rhombohedral, and Cubic. Each of the crystal structures can
>then be subdivided into Simple, Face Centered and Body Centered. And that
>was probably wayyyyy more metallurgy than ya wanted but it makes
>determining the Friday Element Quiz answer much more manageable.
>
>Ir has a Face Centered Cubic (FCC) crystal structure so you get a Mulligan
>and can take a second guess.
>
>Dave
>
>
>
>"Guy Ramsey" <[log in to unmask]>
>04/23/2010 07:45 AM
>
>To
><[log in to unmask]>
>cc
>
>Subject
>RE: [TN] NTC - Friday Element Quiz
>
>
>
>
>
>
>What is a BCC metal?
>I have a guess,
>Iridium, ninth highest melting point, very resistant to corrosion.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
>Sent: Friday, April 23, 2010 8:20 AM
>To: [log in to unmask]
>Subject: [TN] NTC - Friday Element Quiz
>
>Hi folks! Ok, its Friday so its time for another element quiz:
>
>The Question:
> I am a ductile BCC metal and one of the few BCC metals that has
>no ductile-to-brittle transition. My elemental name is part of Greek
>mythology.
>
>Bonus Points:
> Name this metal's greatest attribute and its melting temperature
>rank with respect to all of the metals.
>
>
>I am pretty sure that everyone will be able with some sleuthing to figure
>out which element but the hard part of the question is getting the bonus
>points!
>
>Good luck and again this week, the winner will get to claim Doug's desk.
>
>
>Dave Hillman
>Rockwell Collins
>[log in to unmask]
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|