If your legend is epoxy based it is likely yellowing during the heat
incursion, and making the white ink look off-white. Check temperature and
time in the solder. The size and thickness of the board and its ability to
absorb heat may also be a factor.
Regards
Greg
Triggs
----- Original Message -----
From: "Eric Laroche" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, October 02, 2003 7:43 AM
Subject: [TN] Silk screen changing color
> Good morning Techers,
>
> Does any one have an idea why when I pass a particular board in the
> reflow oven the silkscreen changes to an off white colour? Originally
> the colour is bright white and becomes almost yellow after heat is
> applied to it.
>
>
> Thanks to all,
>
> Eric
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|