TECHNET Archives

May 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Juliano Ribeiro <[log in to unmask]>
Date:
Fri, 18 May 2012 10:31:44 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Message-ID:
Subject:
From:
Rex Waygood <[log in to unmask]>
MIME-Version:
1.0 (1.0)
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
 You are soldering to the PCB finish you do not melt it. ( think of ENIG )

 You are soldering to the PCB finish you do not NEED to melt it. ( think of ENIG )

:-)

Rex

Sent by me on my iPhone. 


On 17 May 2012, at 13:09, "Juliano Ribeiro" <[log in to unmask]> wrote:

> Hi to all,
> 
> Is it possible we use PCB with finishing HASL (Lead Free) in our Tin Lead Process - Solder Wave?
> We need modify some parameters how the temperature?        
> 
> Thank you a lote
> 
> 
> Juliano Ribeiro
> Coordenador de Produção - Placas Eletrônicas 
> Elo Sistemas Eletrônicos S.A.
> Fone: (51) 2131 2217    Fax: (51) 2131 2200
> Cel: (51) 9356 2844                                                                                                                                                                 
> http://www.elonet.com.br 
>  "Antes de imprimir pense na sua responsabilidade com o meio ambiente."
>   Adote os 4 R´s (Reduzir, Reutilizar, Repensar e Reciclar)!
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2