TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wrobel, Clayton" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wrobel, Clayton
Date:
Thu, 6 Apr 2006 15:54:12 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
I have seen failures in hand soldering of no-clean flux.  I doubt this
is your problem however.


I have worked with inverter designs.  Although the nominal voltage is
500 Vrms, the startup voltage can be as high as 1500 rms.  Per IPC
electrical clearance for an uncoated electrical conductor for use below
10,00 feet, 500 Vrms requires 140 mil clearance, 1500 Vrms requires over
400 mils clearance.  This is a MUCH likelier cause of failure


-----Original Message-----
From: Andre Leclair [mailto:[log in to unmask]] 
Sent: Wednesday, April 05, 2006 2:12 PM
Subject: Arching or Current Leakage

We have a customer that has a portion of a circuit which randomly fails.
The circuit is a backlight driver (500volt 6mA). The output caps are
0.100 spacing of the terminals.  The process used is No-clean.  Can the
No-clean contribute to failures of the circuit (ie promote arching or
current leakage across the body of the output caps). ???

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2