TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Date:
Fri, 3 May 2013 13:50:54 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (73 lines)
Thanks Inge 

Rich Kraszewski
(920)969-6075

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Thursday, May 02, 2013 11:35 PM
To: [log in to unmask]
Subject: Re: [TN] Phosphorus Containing Fire Retardants Used in PCB Laminate

Laura & Netters,

go to Dropbox/Technet..../ IC Failures

Phosphorus in IC packages and tantalum caps was a worldwide reliability
issue a number of years ago. I have more about it.

Inge


On 2 May 2013 23:29, Laura J Turbini <[log in to unmask]> wrote:

> Rich,
> I have a reference document on Halogen Free  Flame Retardants in
> Electronics.  I will forward the document to Inge and ask him to place it
> in
> his drop box.
> Laura
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
> Sent: May-02-13 4:52 PM
> To: [log in to unmask]
> Subject: [TN] Phosphorus Containing Fire Retardants Used in PCB Laminate
>
> I am seeing un-usually high levels of phosphates in some IC testing that I
> am conducting and am suspecting the fire-retardant used in the PCB
> manufacture.
>
>         > Can someone direct me to a list of phosphorus based fire
> retardants that could be currently used in laminate construction?
>
>         > Has anyone of you seen this same issue and successfully
> correlated
> it back to the PCB fire retardant?
>
> Thanks in advance
>
> Rich Kraszewski / PLEXUS
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2