Kathie, we use IPA, but we also limit the amount of external flux one can
use to hopefully zero, or just a very light touch. Excessive use of external
flux can cause more problems with solder connections than it helps. IMHO and
38 years of dealing with hand soldering problems.
Ron Dieselberg
Trainer/Auditor
BAE SYSTEMS
Cincinnati Electronics Corp.
[log in to unmask]
-----Original Message-----
From: Lambert, Katherine A.
[mailto:[log in to unmask]]
Sent: Wednesday, March 07, 2001 11:10 AM
To: [log in to unmask]
Subject: [TN] Bench top cleaning of hand soldering
Hi folks,
We're in the process of looking for a solvent to replace the Axarel 2200 and
IPA that we are using for flux removal at hand soldering operations. We are
using RMA flux cored solder and RMA external flux. We have mostly the
standard types of surface mount parts and connectors on organic CCAs.
Nothing terribly exotic - just the basics.
What are you folks using out there in TechNet land?
Thanks,
Kathie Lambert
SMT Process Engineer
Northrop Grumman
Baltimore, MD
410-765-9746
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|