TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 24 Sep 2003 18:11:50 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Hi Wei,
What you and I have said is the same thing.

Werner

In a message dated 09/24/2003 16:39:21, [log in to unmask] writes:
>Hi,
>I think the other important reason to use high-temp solder sphere on CBGA
>is because of the big CTE difference between FR-4 and ceramic. It provide
>more flexible joint. Same
>reason as IBM CCGA packages which use high-temp solder column.
>Wei Wang
>
>Werner Engelmaier wrote:
>> Hi Victor,
>> The reason for high-melt solder balls is the same as for solder
>> columns--thicker solder connections (higher stand-off heights) provide
>higher reliability
>> roughly by the square of the heights. This is well documented--just take
>one of
>> my workshops.
>>
>> Regards,
>> Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2