     Subject:  RE moisture Sensitivity
     Author:   [log in to unmask] at OUT
     Date:  7/1/96 
     
     Olly,
     I would like to read this paper, could you give me a little 
     information on ECTC proceedings.
     
     What organization is it?
     Where can I get information on it?
     How can I find this paper?
     
     I am new to this business.
     Thanks in advance
     
     Amy Skubinna
     Mfg. Engineer
     Manufacturers' Services Ltd


______________________________ Reply Separator _________________________________
Subject: Re: Moisture Sensitivity
Author:  [log in to unmask] at OUT
Date:    6/28/96 3:38 AM


Dirk, have a look at the 1995 ECTC proceedings, for an excellent paper by R. 
Shook and others. From memory, a portion of this paper looked at the moisture 
absorbtion/desorbtion from components that were moved from ambient
conditions to a dry box, a number of times. If you are trying to set up a 
factory policy, I think this will be of use.
     
Regards
     
Olly
     