TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Fri, 31 Aug 2007 13:14:16 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (134 lines)
Other things to consider:
1) How clean are the vias (trapped plating salts)?
2) The smaller the VIP, the smaller the voids
3) Two passes of the squeegee with the paste can jam more paste down
into the vias (of course need to have good gasketing of the stencil to
the board)
4) We have found somewhat less voiding with a thinner stencil, but there
are limit to this because of the requirements of different types of
components.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Macko
Sent: Friday, August 31, 2007 12:53 PM
To: [log in to unmask]
Subject: Re: [TN] vOID IN Micro BGA

I will 2nd that. I have experienced a lot of voiding issues when there
are VIPs on uBGAs as well as other BGAs. Often the VIPs are the same
size whether they are located in a uBGA pad or a larger say 25 mil BGA
pad and consequently, its impact is significant. I am trying to get the
design group to always plug and cap all VIPs so this does not become an
issue.

One work around is to use a 2 mil stencil and paste/reflow the side of
the board with this issue prior to populating any side of the board! The
2 mils of paste helps fill the VIPs as long as they are not too big.
Adding an additional reflow to a non-populated board should not be an
issue but needs to be verified.

Good luck,
- Joe

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Friday, August 31, 2007 9:04 AM
To: [log in to unmask]
Subject: Re: [TN] vOID IN Micro BGA

The presence of vias in the pads causes it. Mind, though, that even such
large voids might not affect a long time reliability of the joints.

Regards,

Vladimir

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of shankar rao
Sent: Friday, August 31, 2007 11:49 AM
To: [log in to unmask]
Subject: [TN] vOID IN Micro BGA

Dear All,
   
  We are getting Large voids  in Micro BGA  on someof the pads having
PTH/via  (greater than 40% in dia) after reflow soldering in one of our
multi layer PCB. We are using ROHS paste and ROHS component.  Can I know
what may be the reason for  these voids
   
  Regards
   
  SHANKAR 


K. Shankar Rao
       
---------------------------------
 Unlimited freedom, unlimited storage. Get it now

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2