Before we go off writing specifcations that make the fabrications people spit and swear, I want to remind all that all immersion plating is self-limiting, and when all the substrate is covered, you stop plating, no matter what temperature, or how long you leave it in the plating bath...
Most fabricators have trouble getting 50 microinches of Tin, and 40 is pretty much the standard...
30 is pretty considered pretty thin..
And, no flat finishes are going to perform as well as HASL, if only because of thickness, nevermind superiority of alloy...
Rudy Sedlak
RD Chemical Company
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
All your favorites on one personal page – Try My Yahoo!
|
|
|