TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Date:
Fri, 8 Apr 2005 13:41:16 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (107 lines)
No problem if you use a hydrochloride activated water-soluble flux!

Brian

Ingemar Hernefjord (KC/EMW) wrote:
> Noone with ideas?
> I've asked specialists at Binghamton too.
> Phil? Ruby? --. ..- -. - . .-. ..--..
> Ingemar
>
> -----Original Message-----
> From: Ingemar Hernefjord (KC/EMW)
> Sent: den 5 april 2005 18:09
> To: 'TechNet E-Mail Forum'; [log in to unmask]
> Subject: RE: [TN] Mousebites...
>
>
> Hi Steve,
> alert experts already online. I have two pictures on Nickel plated AlSiC, chemistry and who did
> it can I not shout out just now, except that it's perfecly free from P, very very 100% Ni. It's greyish,
> dull and matte, and very good for 60Sn soldering, at least speaking wetting. Now, we suspect something
> happens after soldering the glass RF glass beads for SMA. Hermeticity becomes leakers, not gross, but
> enough for rejection. I suspect some kind of fragile interface layers, cross sections indicate that, but
> suspected region is much less than micron thick and hard to study.
>
> When you look at the pics on Steve's mousetrap gallery, what do you think about the very tiny superficial
> items, grains or nanonuggets or columns or how they can be caracterised as...do you think they are pure nickel
> too? Are they atomary bound to the bulk plating or vagabonds that don't take part in the serious solder-nickel
> wedding party? If you bite on a gold dollar you'll have to go through a thin layer of human debris and stuff from
> the underwares first...best I could compare with. Can there be such a 'debris' layer on top of nickel
> plating too, and if so, how do I get rid of it?
>
> The pics are 10k resp 20k magnification.
>
> Crazy q, not optimistic about answer..
>
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]
> Sent: den 5 april 2005 15:45
> To: [log in to unmask]
> Subject: [TN] Mousebites...
>
>
> Mornin' all ya'll!
>
> Came back in this morning and looked at the fabs that I posted about
> yesterday some more. We're going to reject them.
>
> Not just because of the mousebites on the annular pads, but we've
> discovered that there are mousebites all over everything. In some
> cases reducing the trace widths.
>
> Take a look at; "Mousebites 1-4" at:   http://www.stevezeva.homestead.com
> If it were just the annular pads, we might have accepted them. But not with
> them occuring all over the fab like this.
>
> Kind regards,
>
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and confidential to
> LaBarge, Inc.  It is for use only by the individual or entity named above.
> If you are not the intended recipient, you may not copy, use or deliver
> this message to anyone.  In such event, you should destroy the message and
> kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2