TECHNET Archives

April 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Grunde Gjertsen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Grunde Gjertsen <[log in to unmask]>
Date:
Mon, 7 Apr 2014 07:32:13 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
V-0 is better, flame extinguish after 10 seconds and there is no flaming drips, see http://www.ul.com/global/eng/pages/offerings/industries/chemicals/plastics/testing/flame/

BR
Grunde

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tuyen Tran
Sent: 7. april 2014 08:37
To: [log in to unmask]
Subject: [TN] PCB Flammable Rating

Hoping someone can help to explain on Flammable Rating: what is different between UL 94V-1 and UL 94V-0

Thanks you

Tuyen Tran (Ms.)
QAE-Sparton VN

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2