TECHNET Archives

November 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nutting, Phil" <[log in to unmask]>
Date:
Wed, 2 Nov 2016 16:03:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (34 lines)
did you talk to Kester application engineer?
> Hi all,
>
> It has become difficult to find information related to tin/lead wave
> soldering.  We have a table top tin/lead wave solder system that we are
> having difficulty dialing in.  We are running Kester 197 flux and Kester
> 63/37 bar solder and producing thru-hole circuit boards for space
> applications.
>
> I'm looking for typical 0.062" board parameters of top side board
> temperatures after fluxing and before hitting the wave.
>
> Thanks in advance,
>
> Phil Nutting  |  HVP Development Engineer   |  Excelitas Technologies Corp
>
> Lab: +1 978.224.4332   |  Office: +1 978.224.4152
> 35 Congress St, Salem, MA  01970 USA
> [log in to unmask]<mailto:[log in to unmask]>
> www.excelitas.com<http://www.excelitas.com/>
>
>
> [Excelitas R_emailsig]
>
>
> Please consider the environment before printing this e-mail.
> ________________________________
> This email message and any attachments are confidential and proprietary to
> Excelitas Technologies Corp. If you are not the intended recipient of this
> message, please inform the sender by replying to this email or sending a
> message to the sender and destroy the message and any attachments. Thank
> you.
>

ATOM RSS1 RSS2