Jonathan,
Most times when using the Pb95Sn5 alloy I would use a reducing atmosphere
for 'fluxing', at the very least using a nitrogen [<10 ppm Oxygen]
atmosphere. This would allow you to reduce the amount of flux required or
change flux types.
By all means check in with Heraeus. Where are you located?
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of jonathan noquil
Sent: Monday, February 08, 2010 12:47 AM
To: [log in to unmask]
Subject: [TN] Flux Cleaning
Hi All
What is the best flux cleaning agent that can effectively remove flux on
ENiAu bond pads?
We solder a copper strap on the silicon with PbSn5 at 350 degc temperature,
the flux contaminates the bonding pads.
Paste is from Heraues. We used an ultrasonic cleaning equipment.
During Au wirebonding, we have lots of bond off occurences? We tried to do
FTIR on the surface and found some traces of that resin contamination.
Is the flux difficult to remove with flux cleaning agent when it was
reflowed at high temperature?
Thanks
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|