We took a simple approach and sealed the periphery of BGAs with a bead of
silicone adhesive after the conformal coating process.  This worked well.

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Gray, Matthew D HS-SNS [SMTP:[log in to unmask]]
        Sent:   Thursday, May 22, 2003 9:54 AM
        To:     [log in to unmask]
        Subject:        [TN] Conformal Coating Application Method for BGA

        Hello -

        I am requesting feedback to material and processes that have
provided
        environmental performance protection for BGAs and other large array
        packages.  The performance environment of consideration is corrosion
and
        humidity.

        Can users provide particular details regarding application process
spray
        (inclusion of steps used for flood/fill/etc), dip, other, and
material that
        has provided a high amount of coverage and ability to protect
electrical
        connections and components in humidity and salt fog environments.
Ideally,
        these materials are below the parylene step.  All feedback is
appreciated.

        Regards - Matt

        ---------------------------------------------------
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2