Actually folks they are not talking about the termination which is
typically tin or tin/lead over nickel but nickel electrodes. There are a
number of process and material issues involved so get the qual data and
acceleration factors and do a good engineering evaluation.
John At 04:00 PM 6/14/00 -0400, you wrote:
>:)
>
>George, you are a master of understatement! And of course I completely
>agree with you.
>
>Nancy, among other things you need to consider the metals' affinity for
>oxygen and dissolution into solder. I expect our metallurgical friend Dave
>Hillman can provide you with the actual numbers for the above and other
>interesting tidbits that we should keep in mind.
>
>regards,
>Bev Christian
>Director of Electronics Manufacturing
>XLTEK
>
>-----Original Message-----
>From: Wenger, George M (George) [mailto:[log in to unmask]]
>Sent: Wednesday, June 14, 2000 3:17 PM
>To: [log in to unmask]
>Subject: Re: [TN] Palladium > Nickel
>
>
>Nancy,
>
>If I had a choice I'd rather solder to Pd than Ni.
>
>Regards,
>
>George
>George M. Wenger DMTS
>(609)-639-2769 Office (609)-639-3210 Lab
>Bell Laboratories Engineering Research Center Princeton
>Supply Network Solutions FMA / AQA / RCA Lab
>PO Box 900, Princeton, NJ 08524-0900
>Route 569 Carter Rd., Hopewell, NJ 08525
>
>
> > ----------
> > From: Nancy Trumbull[SMTP:[log in to unmask]]
> > Reply To: TechNet E-Mail Forum.;Nancy Trumbull
> > Sent: Wednesday, June 14, 2000 11:13 AM
> > To: [log in to unmask]
> > Subject: [TN] Palladium > Nickel
> >
> > Hi everyone,
> > I've not been on for awhile. We have been doing trial runs for a new
> > product. Then I missed placed my brain and hurt myself by falling out of a
> > hammock. Yes, I know it sounds backwards doesn't it.
> > Any way I'm hoping that this finds all of you health and happy. Because
> > believe me it only takes one study mistake to end it all.
> >
> > Now My Question : Sorry if this has already been addressed.
> > More than likely most or all of you have been using these parts.
> > But this is our first notices of the change over..
> > Our supplier of condenser / ceramic chips has informed us of a coming
> > change.
> > They are telling us that they are changing some of the condenser / ceramic
> > chip from palladium to nickel.
> > I have looked up the different between the element and properties.
> > in my handy little Thomas Pocket ref. So I can see the difference in
> > numbers under elements
> > . And I have noted the difference in the density, Melting and boiling
> > points.
> > But I have to be honest It does not mean diddle squat to me.
> > So I have a lot of questions and need a lot of help.
> > As
> > 1. Performance durability
> > 2. Structural difference that might give us issues now and in
> > the further.
> > 3. The reliability of the part it is worst or better.
> > 4. Are these parts already out there , so I really have no
> > worried at all.
> >
> > If someone would be so kind to give me items that I do or
> > don't need to worried about , with reason why. I will greatly appreciate
> > it.
> > My understanding is this is all happening because of the availability of
> > palladium and cost.
> > I thank all of you for taking the time to read my e-mail and those of you
> > that can and will help me out.
> > Nancy T.
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information.
> > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > ##############################################################
> >
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|