TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Rex Waygood <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Date:
Tue, 30 Apr 2013 17:13:46 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (85 lines)
And probably has no detrimental effect on reliability.
Rex

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: 30 April 2013 17:05
To: [log in to unmask]
Subject: Re: [TN] Pic of head-in-pillow for the site

Thanks, Steve.

That void measures < 25%. Not optimum, but conforms to IPC-610 Class 2.

Ed Popielarski
Engineering Manager

[Description: FullLogo]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A

From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 30, 2013 8:55 AM
To: Ed Popielarski
Cc: [log in to unmask]
Subject: RE: Pic of head-in-pillow for the site

Hi Ed!

Nice image! Got it posted, it's here:

http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG

What about the void off to the right? Is there any concern about that?

Steve Gregory
Process Engineer
Kimco Design and Manufacturing
652 N. Five Mile Road
Boise, ID 83713
(208) 322-0500 Ext. 3133

From: Ed Popielarski [mailto:[log in to unmask]]
Sent: Tuesday, April 30, 2013 8:58 AM
To: Steve Gregory
Subject: Pic of head-in-pillow for the site

Hi Steve,

I have a good X-Ray picture of a head-in-pillow that Leland would find
helpful. If you don't mind posting it for him?

Ed Popielarski
Engineering Manager

[Description: FullLogo]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________