TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Mon, 30 May 2005 09:00:10 +0200
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guenter Grossmann <[log in to unmask]>
Subject:
From:
Guenter Grossmann <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (38 lines)
Ken

No I haven't read a paper, but these microcracks are frequently seen in
our lab in failure analysis. They occur due to 3 reasons (as far as I
know):
- 2 Solidification fronts meeting each other and being already too cold
to join. I believe that this is mainly a design problem.
- Shrinking of the rest- eutectic between the Sn dendrites
- Well I believe that a SnBiPb rest- eutectic is rare nowadays

Best regards

Guenter



EMPA
Swiss Federal Laboratories  for Materials Testing and Research
Centre for Reliability
Guenter Grossmann,  Senior Engineer

8600 Duebendorf
Switzerland

Phone: xx41 1 823 4279
Fax :     xx41 1 823 4054
mail:     [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2