TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Tue, 22 May 2001 06:57:09 -0500
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Rob Day <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
You could try Winslow Automation.  They have some good methods.  We found an outside source in our local area (NH) that has great turnaround and is very reasonable.  You could try that route too.  We have found that that works best for us.

Rob Day

>>> [log in to unmask] 05/22/01 01:18AM >>>
Hi all,
I  got few questions about reballing the BGA.
1. If I want to re-ball the BGA, so what's alloy should use for the balls???63/37 or 60/40 or ....
2. what's method should i use to placing the balls on the BGA if the balls are in loose form ???
3. what ' s profile should I use for reflow the BGA's???
Thanks for your help
Van 
[log in to unmask] 

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2