Thomas Kropski wrote:
> 
> What is the smallest reasonable text size for silkscreen text. Text
> height, width, and thickness. With design density increasing, we would
> still like to have as many ref des possible.  From a PCB designer,
> what tooling parameters are acceptable for good resolution on the
> finished products.


The only real limitation to silkcreen is your PCB fabricator. We have
successfully used 40 mil high by 6 mil stoke width with the right
vendor. Older eyes may require help, but the text is completely readable
and clear. Our typical text size is 60 x 10 and 50 x 8. Our software
does not control the width.

As to the suggestion of eliminating silkscreen altogether by Tom Coyle,
that is a tempting but limited view. Every company will have different
products and priorities. Saving $1 per panel could cost $thousands in
assembly and rework errors. If your engineers get everything right every
time, and you use pick and place machines for assembly with every single
part, including through-hole parts on both sides of the PCB, and do not
add discrete wiring at a later assembly, who needs silscreen? :)

David

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2