Thomas
We had this problem on an older model Hollis machine, oh - around 20 years ago. This machine, as I
remember, had bottom side heaters. I figured that the expansion of the hot solder at the bottom of the pot
builds up enough pressure that it eventually finds a weak spot in the cooler upper crust and then it does
it's Mt. St. Helen imitation. We manufactured a cover that covered the pot and conveyor chain and just let
her spit up every morning.
We have never seen this problem on our newer Hollis machine because it has side heaters that melt the
solder top to bottom, thus giving the expanding solder relief. I suppose a cartridge heater could be
mounted at a side location to similarly create a vent for bottom heated machines.
Gary Camac
Thomas C Han wrote:
> Hi all,
>
> Our solder on the Technical Devices wave solder machine is set to come on
> at early morning so that by the time my operators come in for work,
> solder pot will be at its set temperature. My operators have noticed
> solder splatters along the conveyor rails and vacinity around the solder
> pot. I think it happens during heating of the solder pot. Do you have
> any ideas as to what would cause the solder pot to splatter during
> heating?
>
> Your input is greatly appreciated
>
> Tom Han
> Ardent Systems
>
> ___________________________________________________________________
> You don't need to buy Internet access to use free Internet e-mail.
> Get completely free e-mail from Juno at http://www.juno.com
> or call Juno at (800) 654-JUNO [654-5866]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|