TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Date:
Wed, 8 Mar 2006 06:39:11 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (AZ75)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Whittaker, Dewey (AZ75)" <[log in to unmask]>
Parts/Attachments:
text/plain (135 lines)
Is that before or after you do the Cajun down there.
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, March 07, 2006 3:27 PM
To: [log in to unmask]
Subject: Re: [TN] ESD and paintbrushes

Great! They have the "Roadkill Law" in Louisiana and it's legal to take
what you hit home to eat (or in this case, make paintbrushes).


Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, March 07, 2006 4:00 PM
To: [log in to unmask]
Subject: Re: [TN] ESD and paintbrushes

At last here comes my million bucks.

Jason I will cut you in...............round up all of those nutria and
we will make a bundle exporting them to China where all of the assembly
is being done................8-)

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, March 07, 2006 1:18 PM
To: [log in to unmask]
Subject: Re: [TN] ESD and paintbrushes

I read somewhere that only Llamas and Nutria (the rodents that live all
over
Louisiana) have ESD safe hair.


Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Tuesday, March 07, 2006 2:59 PM
To: [log in to unmask]
Subject: [TN] ESD and paintbrushes

OK, I have not asked a stupid question all day, so I am due.

We do a fair amount of conformal coating by hand, using artist brushes.
Would you consider paintbrushes with soft nylon bristles to be ESD
hazards and if so, why?

Doug Pauls

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2