TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 9 Oct 2001 16:33:13 +0100
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
From:
Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (89 lines)
Agreed the limiting factor is likely to be pad adhesion: did some work in
this area a while ago which indicated you could rework the pads or at least
copper foil same thickness as the pads >8 times, but that in real world
unsupported pads (i.e. no though connection etc) would consistently unstick
after around 4-5 goes. This was very much a pragmatic exercise just to
determine an order of size, too many real world variables with arbitrary
numbers to give a scientific answer. These numbers would be lower now as pad
sizes have decreased

Best regards

Mike Fenner
Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask]
W: www.indium.com
Leadfree: http://Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Collins
Sent: Tuesday, October 09, 2001 4:17 PM
To: [log in to unmask]
Subject: Re: [TN] # of rework cycle for SMT gullwing component


Moonman - when I worked for Celestica (Toronto) we only allowed 2 for any
surface finish.  I worked both HASL and OSP.  I believe there was more
concern with pads lifting than intermetallic layer.  Besides - if you have
to replace a part 3 times you have some serious issues to work.

regards

Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215

>>> [log in to unmask] 10/08/01 03:53PM >>>
For fine pitch and BGA, HP and Celestica used to allow two cycles for HASL
(ring a ding) and three for OSP and ENIG. Why is that?

MoonMan

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2