TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Douthit <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 16 Sep 2003 17:42:11 -0700
Content-Type:
multipart/alternative
Parts/Attachments:
text/plain (2556 bytes) , text/html (3793 bytes)
Steve,

You might consider the fact that metal will change temperature much
faster than polymers.
This thermal gradient "split" can cause serious temporary CTE
mismatches.

David A. Douthit
Manager
LoCan LLC

Steve Gregory wrote:

> Yep, got the tape and used it on this part...I've always used it on
> parts with a heatsink. The profile I had was basically the same
> profile I've used with a Analog Devices SHARC 240-pin QFP that has a
> heatsink in the top like this Altera part.
>
> I wonder if I should be concerned with other parts from this lot, even
> if they've not exhibited the cracking like this one part did?
>
> -Steve Gregory-
>
>
>
>> Do you have that Black TyveK tape? PDR gave us some for use with
>> metal case components. I think that metal top may reflect more
>> energy than the black plastic. I bet the temperature difference is
>> enough to crack the package. It might be lot dependent, There is
>> probably some variation in the actual thickness of the plastic over
>> the metal spreader. I don't think this was due to moisture.
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------


ATOM RSS1 RSS2