TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 5 Jun 1997 10:42:06 +0200
Precedence:
list
Resent-From:
From [log in to unmask] Thu Jun 5 16:
42:06 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13178
>From bergdi Thu Jun 5 03:
23:37 1997
X-Sender:
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"JQvpN1.0.4QA.pTdbp"@ipc>
Subject:
From:
[log in to unmask] (Guenter Grossmann)
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wZXpF-000BjMC; Thu, 5 Jun 97 03:23 CDT
Message-Id:
<v01520d00afbc21ba4d3d@[129.132.54.198]>
Parts/Attachments:
text/plain (38 lines)
Tony

Thanks for this report. It makes me feeling a bit better. Some months ago I
had to compile layout rules for SMT and I based them on calculations Dieter
Bergman presented back in 1992 ( now in IPC-782 ? ). However I didn't trust
the spec ( that's the way we scientists are ). I recalculated the land
pattern for a tantalum capacitor type "B" with the formula for the elastica
of eutectic solder in air. The result was astonishing and I nearly didn't
dare to show it to our industry partners. Unfortunately there was no more
money in the project to verify the results. Anyway here are the results:

Pad size reflow: Z = 5.6mm; Y = 0.99mm; W = 2.61mm
Pad size wave: Z = 12.2mm; Y = 0.99mm; W = 2.61mm

Z = Overall outside distance of pads
Y = Inside distance between pads
X = With of pads

which results in  4mm exposed land. Of course, the elastica applies only to
a laminar wave. I wish I had the founds to evaluate a correction factor for
turbulent waves.

Best regards

Guenter Grossmann


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2