TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Roland Jaquet <[log in to unmask]>
Date:
Thu, 24 May 2007 12:30:55 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Herminia Guevarra <[log in to unmask]>
Subject:
From:
Herminia Guevarra <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<001001c79e1e$85d450c0$2701a8c0@HPNW8440RJ>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (282 lines)
Hi, Roland,

Here attached from Inge...

Thanks,

Herminia 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roland Jaquet
Sent: Thursday, May 24, 2007 12:14 PM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

May I too, if you please

Meilleures Salutations
Very Best Regards
Roland
 
www.PCBspecialist.com 
Roland Jaquet
14 Champ Budin
1258 Perly, GENEVA
SWTZERLAND
TEL+41-22-880-0405 GSM+41-79-203-3723 FAX +41-22-880-0409
There are three constant in life... Change, Choice & Principles.
Stephen R. Covey
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Lee parker
Envoyé : jeudi, 24. mai 2007 16:35
Ā : [log in to unmask]
Objet : Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

Herminia

Please send me a copy.

Thanks

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389




----- Original Message ----- 
From: "Herminia Guevarra" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, May 24, 2007 8:54 AM
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder


Vielen Dank!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Thursday, May 24, 2007 8:00 AM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

Naturalmente..lo me parece muy bien
Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Herminia Guevarra
Sent: den 24 maj 2007 13:23
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

I'm also anxious to have this report.  Please include me...

Herminia

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Frederick Miller
Sent: Thursday, May 24, 2007 7:55 AM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

Add me to the list.
Fred

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Victor G. Hernandez
Sent: Wednesday, May 23, 2007 4:17 PM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder


I would like to view this presentation/report.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Wednesday, May 23, 2007 3:16 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] SV: [TN] Definition of Eutectic Solder

Richard, George, Werner etc chief gnus,

Want a very advanced article on the theme SAC, IMC, Phosphorous rich Ni, 
diffusion rate, solidifying, wetting, ENIG, crystallographic pictures, SEM 
pictures, etched cross sections, X-ray investigations, microprobing...more 
than 30 pages?

I made a consulting job (metallurgists, need assistance) and had a two hours

presentation of my job. Both companies were satisfied, much thanks to advice

from you, but also thanks to my collegue, who is from Beijing.
He gave me a report that lifted my eyes. I've never seen SAC/ENIG cross 
section presentations like that. Not even from China Lake. Can send offline 
if you are not too many. Please, be aware this is not a popularised kind of 
presentation, but at a advanced metallographic level. You may have it 
already...don't know, but the report is fresh.

Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier
Skickat: den 23 maj 2007 20:44
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] Definition of Eutectic Solder

Hi Richard,
If you try to solder at or just above the Solidus temperature, you need a 
long time to get wetting [it takes thermal energy to dissolve the base metal

into Sn], and you may not get good wetting art all. That is why I recommend
Liquidus+20C for reflow soldering to Cu, and Liquidus+35C for reflow
soldering to
Ni. This time above 183 recommendation of 60 to 90 sec is wrong.



Werner



**************************************
 See what's free at http://www.aol.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2