Pearl what hit that a truck?
Only thing I am having trouble understanding is the bends on the two leads
on the right (the two on the left are also looking broken at the pad
interface.)
The bends on the 2 interconnects on the right suggest that the side that we
were looking at was forced mechanically up in the Z axis, the two traces on
the left broke off at the pad interface while on the two on the right the
trace came up with the pads and the z axis force was then removed causing
that bend in the trace.
I would bet a lunch on all four pads we are looking at being delaminated
from the laminate underneath.
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, February 02, 2010 3:11 PM
To: [log in to unmask]
Subject: Re: [TN] track lifting
Hi Pearl,
Here's your picture:
http://stevezeva.homestead.com/files/Track_Lifting.JPG
What I see in the picture is that BGA (it is a BGA isn't it?) was almost
ripped-off the board somehow.
The traces are stretched and the soldermask has been torn up from the board.
The root cause is that something mechanically hit the BGA and ripped up pads
and traces. Is there any other marks on the BGA?
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of pearl petras
Sent: Tuesday, February 02, 2010 5:13 PM
To: [log in to unmask]
Subject: [TN] track lifting
While we wait for IPC to set up a picture site, could I impose on Steve to
post another picture?
Any comments as to what could possibly be the root causes of this is much
appreciated.
Thanks so much
__________________________________________________________________
Yahoo! Canada Toolbar: Search from anywhere on the web, and bookmark your
favourite sites. Download it now http://ca.toolbar.yahoo.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|