Parts/Attachments:
text/plain (199 lines)
Contact your fab supplier with this picture.  The spring test probes in the
area where this picture is taken are applying too much force.
It must be in an area with more than one BGA, or an area heavily populated
with test points.

Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
825 University Avenue
Norwood, MA 02062-2643
(T) 781-467-5468
(C) 508-631-1832
(F) 781-461-0993
|-----------------------------+-------------------------------------------|
|   Steve Gregory             |                                           |
|   <[log in to unmask]                                           |
|   OM>                       |                                         To|
|   Sent by: TechNet          |                                        Tec|
|   <[log in to unmask]>         |                                        hNe|
|                             |                                        t@I|
|   08/07/2007 08:26 AM       |                                        PC.|
|                             |                                        ORG|
|         Please respond to   |                                         cc|
|       TechNet E-Mail Forum  |                                           |
|        <[log in to unmask]>;   |                                    Subject|
|         Please respond to   |                                        Re:|
|           Steve Gregory     |                                        [TN|
|      <SGregory@OAIELECTRONIC|                                        ]  |
|              S.COM>         |                                        Den|
|                             |                                        t  |
|                             |                                        on |
|                             |                                        BGA|
|                             |                                        Pad|
|                             |                                           |
|                             |                                           |
|                             |                                           |
|                             |                                           |
|                             |                                           |
|                             |                                           |
|-----------------------------+-------------------------------------------|






Hi Again Amol!

I have your picture posted. It's at:

http://stevezeva.homestead.com/files/Dent_on_BGA_Pad.jpg

That looks like an awfully deep probe mark to me. Yes, something like
that will cause voids.

I did find this in the IPC-6012A with Amendment 1 - Qualification and
Performance Specification for Rigid Printed Boards on page 10:

3.5.4.2

Surface Mount Lands - Defects such as nick, dents, and pinholes along
the edge of the land shall not exceed 20% of either the length or width
of the land for Class 2 or Class 3 boards, or 30% for Class 1. Defects
internal to the land shall not exceed 10% of the length or width of the
land for Class 2 or Class 3 boards, or 20% for Class 1.

That sure looks like more than 10% to me...

Kind regards,

Steve Gregory
Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112

(918) 836-9077 ext 507
(918) 836-0184 FAX

-----Original Message-----
From: Kane, Amol (349) [mailto:[log in to unmask]]
Sent: Tuesday, August 07, 2007 6:52 AM
To: Steve Gregory
Subject: RE: [TN] Dent on BGA Pad

Thanks Steve, here it is


Amol S. Kane
Process Engineer
Harvard Custom Manufacturing
941 Route 38
Owego, NY 13827

Phone: 607-687-7669 Ext. 349
Fax: 607-687-9733
Email: [log in to unmask]


-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, August 07, 2007 7:49 AM
To: Kane, Amol (349)
Subject: RE: [TN] Dent on BGA Pad

Good Morning Amol!

Just go ahead and send it to me and I'll post it for you, then send you
a link to the photo.

Kind regards,

Steve


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Tuesday, August 07, 2007 6:42 AM
To: [log in to unmask]
Subject: [TN] Dent on BGA Pad

Dear Technetters,
Lately, we have been receiving bare boards from our supplier with some
dents on the BGA Pads (ENIG Finish). The dent is plated too (no exposed
Ni). What kinds of assembly defects can potentially be associated with
this condition? (voiding and coplanarity post reflow comes to mind). Are
there any specs that cover this kind of condition/defect? I want to
reject this board but need something to stand by

I am sure that somebody else has seen this too, how was this dealt with?

Steve: I wish to post a picture of this condition, can you please direct
me how to do it?


Thanks in advance,
Amol

------------



CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2