TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Fri, 31 May 2013 11:09:43 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Douglas Pauls <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (170 lines)
Nah.  More along the lines of having something wonderful/valuable grow out 
of something that starts as an irritant.  Kind of like our friendship 
<grin>.

Doug Pauls



From:   "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
To:     TechNet E-Mail Forum <[log in to unmask]>, 
"[log in to unmask]" <[log in to unmask]>
Date:   05/31/2013 11:06 AM
Subject:        RE: [TN] PCB RELIABILITY ENGINEERING



I resemble that remark. Your reference to "pearls of wisdom" was a 
reference to the mingling of the cultured and un-cultured.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, May 31, 2013 9:01 AM
To: [log in to unmask]
Subject: Re: [TN] PCB RELIABILITY ENGINEERING

Yes, I did catch that.  But as you indicate, the IPC has an office in 
India.  And while the asker may not be able to physically attend the 
meetings, we are starting to get more connected now that WiFi is 
everywhere.  A LOT of standards specification work is being moved along by 
Webex or similar web-based meetings, so participation in IPC should not be 
based on whether you can physically make the meetings. 

Yes, the after-meeting stuff would be much more fun if you attended.  I 
guess the point being is that a lot of networking goes on outside of the 
meetings and you get the priceless pearls of wisdom often through such 
networking.

Doug Pauls



From:   Karen Tellefsen <[log in to unmask]>
To:     <[log in to unmask]>
Date:   05/31/2013 10:53 AM
Subject:        Re: [TN] PCB RELIABILITY ENGINEERING
Sent by:        TechNet <[log in to unmask]>



Good response, except the asker has an email address that suggests he 
lives in India, and may be unlikely to go to US IPC meetings. 
Also, not everyone goes out for beer and pizza after the meetings, I 
usually don't. 

IPC has an office in Bangalore, some of my Indian colleagues attend their 
meetings. 
http://www.ipcindia.org.in/html/default.htm

Karen Tellefsen - Electrical Testing
Alpha / 109 Corporate Blvd./ S. Plainfield, NJ 07080 [log in to unmask]
908-791-3069




From:   Douglas Pauls <[log in to unmask]>
To:     <[log in to unmask]>, 
Date:   05/31/2013 11:22 AM
Subject:        Re: [TN] PCB RELIABILITY ENGINEERING
Sent by:        TechNet <[log in to unmask]>



You ask a question far too broad for a reasonable answer.  As a start, I 
would recommend any books by the late Dr. Werner Englemeyer, an active 
participation in Technet until his death.  You can search on the Technet 
Archives using his name as a keyword and probably still be reading this 
time next year.

Are you talking about reliability of the bare board or of the finished 
assembly?  Two very different things, but related.

Brian Ellis's text on cleaning should be on everyone's desk.

Clyde Coombs has authored an excellent reference book "Printed Circuits 
Handbook", published by McGraw Hill.  Mine is the 5th edition but it might 



be up to the sixth edition by now. 

Charlie Harper has a good book, Electronic Materials and Processes, also 
McGraw Hill, 6th edition.

Beyond that, it depends on what aspect of reliability you are looking for. 



 

I will say though, that if you really want the best education in 
electronics reliability, stuff you won't find in most books, get involved 
with the IPC standards and attend what meetings you can.  I can't begin to 



tell you the education it has provided me over the years.  You learn as 
much over pizza and beer after the meetings as you do in the meetings 
itself.

Doug Pauls



From:   Ramakrishnan Saravanan <[log in to unmask]>
To:     <[log in to unmask]>
Date:   05/31/2013 09:43 AM
Subject:        [TN] PCB RELIABILITY ENGINEERING
Sent by:        TechNet <[log in to unmask]>



Dear All,

Which book should i study to understand the reliability engineering of 
PCB. regards,


R.Saravanan




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




***** Please note that my E-Mail address has changed *****

____________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please visit http://www.symanteccloud.com
____________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2