Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vnlp0-0000TtC; Fri, 24 Jan 97 07:37 CST |
Old-Return-Path: |
|
Date: |
Fri, 24 Jan 97 05:47:08 PST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Fri Jan 24 09: |
09:57 1997 |
Resent-Message-ID: |
<"jmsFm2.0.gJ7.UiBwo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Most "clear" soldermasks are slightly cloudy or not crystal clear. It
is due to the fillers etc. Although with out seeing the board I do
not know if it is less or more hazy then "normal."
The line of ending up "crystal clear after mass soldering" is most
likely not true. If anything soldermasks in general become more
cloudy after assembly because of interactions with flux. But if
Dynachem believes this ask them to prove it to you! I would love to
see the results.
Good Luck
______________________________ Reply Separator _________________________________
Subject: FAB: Clear LPISM
Author: [log in to unmask] at corp
Date: 1/23/97 4:06 PM
When using Epic LPI soldermask, clear color, our finished bare boards
have a slight "haze" left in the finish. We've been told by Dynachem
and some of our customers that this is normal and usually ends up
crystal clear after mass soldering. Other customers of ours query the
"cloudiness" or "haze" in the finish.
Any help substantiating the normality or abnormality of this
would be much appreciated.
Thanks....John Gordon
LANmark Circuits, Inc
(916)272-7280
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|