Hi Pete,
If the PCB had thin, porous gold, you may have not seen it visually after the first reflow. But after the board goes through the wave the gold gets leached off and the non-wettable, oxidized nickel would be exposed.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Friday, June 10, 2011 9:59 AM
To: [log in to unmask]
Subject: Re: [TN] Black Pad?
The second batch of pictures showed a lot more black pad/tar/whatever. So now I'm curious - if it is oxidized Ni, from black pad or any reason, shouldn't it have appeared prior to the wave process that couldn't wet?
Pete
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|