----Thanks to everyone for the info , I was a weak on Cupric, (I spent
my life using mostly Ammonium and Ferric, amongst other more exotic
etches)
Any way one more simple or not so simple question :
Would you run a Cupric etcher @ 140g/l Cu and 5N HCl .?
Is It a correct assumption that somewhat lower N, and higher
copper would , provide faster etch rate. It just seems to me that
operating at an extreme N will basically just cost money in the form of
excess HCL usage , not to mention the wear and tear on the equipment,
and operators.,
Again thanks for the information!
Russell Smith
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|