TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 12 Mar 2009 15:13:46 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Parts/Attachments:
text/plain (65 lines)
Chris:
The exact formula is not critical, do not sweat it, pick mid values and go with it.
BUT, do realize this stuff is NOT mother's milk, and in fact, could corrode virtually any metal except 300 series stainless steel, and will react, perhaps in an "exciting way", with organics spilled into the bath. 
The big advantage of the Dow Corning stuff it is so benign, and won't corrode, or react in exciting ways.

Rudy Sedlak

--- On Thu, 3/12/09, Chris Mahanna <[log in to unmask]> wrote:
From: Chris Mahanna <[log in to unmask]>
Subject: [TN] Bath Salts
To: [log in to unmask]
Date: Thursday, March 12, 2009, 1:20 PM

Hello all,

Does anyone know if there is extra fairy dust in bath salts (other than
anticake and pink food coloring)?  For that matter, what's anticake?

I need to run liquid thermal shock testing at 300C.  We've been using Dow
Corning 710.  In an open system, kinda cost prohibitive.

I gather from MSDSs that we can mix a eutectic somewhere around:

Potassium Nitrate: 40-50%
Sodium Nitrate: 10-20%
Sodium Nitrite: 30-40%

Extra credit to any mixing experts that know the exact formula for ~200-350C.

I can source the salts a couple blocks away for $, or the mix from across the
country for $$$$$.
I'd much prefer going down the street.

Thanks!

Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
      

ATOM RSS1 RSS2