Bob,
I don't think this will help, if the contacts are rubbed down to laminate level....
But RHODIUM plating has been used in high wear applications....better than Au.
We used to have Rhodium bath....not anymore.
Rashesh
www.accueng.com
818-768-3919
-----Original Message-----
From: bob wettermann <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Mar 16, 2010 6:53 am
Subject: [TN] Gold Finger Plating for High Vibration Environments
Dear Technetters:
We are trying to advise a client on PCB specifications for a future product
build. These boards are heavily weighted down with water-cooled heat sinks
and heavy transformers. In the end use environment the boards are
vibrated under load and eventually the hard gold 4 um thick goldfinger
contacts are rubbed down to the laminate level.
Besides a mechanical redesign any other plating surfaces anyone would recommend?
Thanks!
Regards
Bob Wettermann
BEST Inc
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|