Hi There,
Pd was first proposed as an alternative to acid hard gold. The argument was
that at the time it was approx 1/2 the gold price and coincidentally about
30% less in density (ie more micron per unit mass).
The origional claims about equivalent electrical contact resistance proved
unfounded and the compromise of high Pd plus flash gold came up.
I imagain you are looking for bonding properties wherein I would argue
electroless, pure gold would be much better than Pd. Incidentally Pd is now
2.5 X the price of PD!!!
Best Regards,
Ken Mc Gowan
----- Original Message -----
From: "Jean-Luc Lehmann" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 15, 2001 1:28 PM
Subject: [TN] PCB paladium plating
> A PCB supplier propose paladium plating. The statement is that the
> surfacing is as good, if not better, than gold plating (for SMD) without
> the need for Nickel plating.
> Also manual soldering needs some extra flux because the tip does not get
> enough heat contact (surface too flat and hard).
>
> What are the pros and cons of paladium finish on PCB ?
>
> Jean-Luc Lehmann
> Project Manager
> DPS S.A., CH-1217 Meyrin
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|