TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Goodyear, Patrick" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Goodyear, Patrick
Date:
Tue, 16 Apr 2013 22:25:52 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (142 lines)
Bob, 

I think they rode an elevator to 1500', so they only climbed a 268 foot tower!!! LOL    260 was bad enough, considering the wind here blows at 20Knots at 10 in the morning you have to climb before coffee.   Thankfully I am toooo old to climb any more.   

Pat   

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
Sent: Tuesday, April 16, 2013 1:27 PM
To: [log in to unmask]
Subject: Re: [TN] Butane Soldering Irons

Aww that's not so hard - look what these guys can do

http://www.youtube.com/watch?v=jbEqnLjHyf8 (1768 foot tower climbing)

http://www.youtube.com/watch?v=mozYoPICQJE

http://www.youtube.com/watch?v=AHe3mRo4jGw

Bob L.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Tuesday, April 16, 2013 1:58 PM
To: [log in to unmask]
Subject: Re: [TN] Butane Soldering Irons

Pat,

I prefer to be in my powered parachute at 250 ft AGL, rather than hanging on a tower ....  although at 10 kts, I would likely still be on the ground.

Sometimes you just have to use what you have to use.  It may not be ideal, but it better than nothing!

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Tuesday, April 16, 2013 11:28 AM
To: [log in to unmask]
Subject: Re: [TN] Butane Soldering Irons

Sorry for the late reply but I just got back from vacation.  
So I have had the need to perform soldering using a butane powered soldering
iron, wasn't ideal but it did work quite well.   Here was the scenario, 250'
in the air on a Meteorological tower soldering a four conductor connector for an RTD onto the cable going down the tower, a 10Knot wind at 50 deg.F blowing off of the ocean 400 feet below.  No AC power available, the cordless irons ran out of battery before the joint was hot enough to get
good wetting.   We tried a 100 watt battery operated gun and that also
didn't work very well tip was the size of a pencil.  So out comes my butane solder torch with the medium size tip, it worked amazingly well the hard
part was getting it lit, the wind kept blowing out the lighter.   We used a
large paper cup as a wind screen, poked the connector in the bottom.
Soldering with gloves on is not easy.  

I use the small butane torch quite a bit for sliver soldering, I think the melt is around 1200 deg., but I don't use the solder tips only the flame in
that case.   

Pat    

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Friday, April 05, 2013 10:12 AM
To: [log in to unmask]
Subject: Re: [TN] Butane Soldering Irons

I have a couple of these, very handy for working on my old car and odd jobs.
The problem with them for anything serious is that the tip temperature is not well controlled. 
1) The heat output from the catalytic combustion heater is not calibrated; it can be set to anything. Probability is that it will end up on max, because when things don't work in soldering that's what people do.
2) the overall design is geared to a quick warm up, so there is little thermal mass, this will allow big temperature variation with more than one joint or if the work requires  long heat time because of its own thermal mass.
3) The bit is a screw on type and this gives poor thermal coupling especially after some period of use.
The reason I have two, is that the first one had these problems in spades, the second I paid a lot more for. It is better, so I can solder up my old car wiring and stuff like that just fine. For circuit board work they make me nervous.
Cordless irons tend also to go for a high temp, low mass, quick warm approach. 
Need to think in terms not just of temperature but the amount of heat available. A lot of heat is not the same as a high temperature.

So overall it means you would be putting a high premium on operator skill.
IT would be worth going to some trouble to avoid them. 
For example low voltage irons that could run from a car battery.
Alternatively an inverter so you could use a regular iron.
Example: for my bush camping trips I just have a small inverter which generates 140W mains output. It's the size of a small apple and plugs in to car socket and cost about 50USD. Probably less in USA. Saves buying a separate charger for each piece of kit and doesn't become obsolete if I up grade anything.
So one of those with a mains extension cord could do it I think.

Regards

Mike


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Owens
Sent: Thursday, April 04, 2013 3:38 PM
To: [log in to unmask]
Subject: [TN] Butane Soldering Irons

Since we hand solder outside of the normal manufacturing floor, our technicians are requesting to use a butane soldering iron. I have no previous experience with this type of soldering iron. With a temperature setting of 1076°F it seems rather high and potentially damaging to resulting solder connection, insulation, people, etc.

http://www.apexhandtools.com/brands/CF_Files/model_detail.cfm?upc=0371030609
76

Any thoughts from experience would be most appreciated.

Gregg

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2