TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Michael Sewell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Michael Sewell <[log in to unmask]>
Date:
Wed, 28 Sep 2005 10:12:28 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (190 lines)
                                Not to mention that the .050" core makes a good shield when x-rayed with the BGA on the top side, which is why we were turning the Kv up anyway.   Now, if its on the bottom side during x-ray and nearly flush to the x-ray source.....

                                Mike Sewell




        Franklin Asbell <[log in to unmask]>
                        Sent by: TechNet <[log in to unmask]>
                        09/28/2005 09:16 AM
                        Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Franklin Asbell <[log in to unmask]>
                                	
        To:     [log in to unmask]@SMTP@Exchange
        cc:     (bcc: Michael Sewell/LABARGE)
        Subject:        Re: [TN] X-ray inspection damaging components...	


                                My first question at such a technical meeting would be

                                How much exposure will damage the part?

                                I'm sure if you place the part in the chamber, turn on the xray and go to
                                lunch you might have some problems. But would seconds, cause damage?

                                What might be happening is component vendors want to protect their product
                                and obviously so, so they place tighter than required standards on them,
                                what is the time to failure under 90kv at 20mA, and at 50mA, and at 90mA?
                                What is time to failure under 40kv at 90mA for 5 seconds? Or 30 seconds?

                                Just some things I would try to answer during such an IPC technical
                                activity.

                                Franklin



                                -----Original Message-----
                                From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
                                Sent: Wednesday, September 28, 2005 9:01 AM
                                To: [log in to unmask]
                                Subject: Re: [TN] X-ray inspection damaging components...

                                 Good Morning, Stephen!
                                This is good information. So now we have component vendors telling us
                                some of their components should not be overexposed to X-rays. Was there
                                any type of notation on the part print?
                                The industry needs a standard. We need to have some type of rating
                                system for components that can be damaged by X-rays.
                                Jack, is there any activity going on with this within IPC?

                                -----Original Message-----
                                From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
                                Sent: Wednesday, September 28, 2005 8:50 AM
                                To: [log in to unmask]
                                Subject: [TN] X-ray inspection damaging components...

                                Morning All!

                                I submitted a question to Altera via their email support center about
                                x-ray inspection possibly damaging a EPM7256EEFI100-7 device. The device
                                is a EEPROM made using an advanced CMOS process.

                                Here is our exchange so far:

                                >Request No: 10515187 Status: Close-Pending Date Opened (PDT): 9/26/2005

                                >07:24 AM Date Closed (PDT):
                                >Inquiry Type: Product Question
                                >Device Family:   Device:
                                >Title: X-ray inspection of devices
                                >
                                >Description: I am doing x-ray inspection of a EPM7256AEFI100-7 device
                                after board assembly.
                                >The PCB has a 1.27mm thick copper core in the center of it, so it
                                >requires
                                that a high kv x-ray must
                                >be done in order to see the solder connections of the device. The x-ray
                                source power is around
                                >120-130kv. Will this x-ray power level damage the device?
                                >
                                >Thank-you,
                                >
                                >-Stephen Gregory-
                                >Process Engineer
                                >LaBarge Inc.
                                >
                                >
                                ------------------------------------------------------------------------
                                --------------------
                                >
                                >Updates  1 - 2 of 2  Add an Update / Previous / Next
                                >
                                >Date Created (PDT) 9/27/2005 07:44 PM
                                >
                                >To Customer:
                                >
                                >Hi Stephen,
                                >
                                >Typically assembly uses 90KV using 10 to 20mA with a few second for
                                inspection of IC package. Our
                                >recommendation will be a pro-rated 130KV with 7mA to 13mA for a few
                                second. Note that Prolong exposure
                                >under X-ray will definitely damage the device. I hope it's helpful to
                                you.
                                >
                                >Best Regards,
                                >Daniel Cao

                                My question is; doesn't the figure of 90KV at 10-20mA seem pretty low?

                                My current Glenbrook RTX-113 operates at 35-52KV at 20-50mA, and
                                higher-end Glenbrook systems will pump 70-90KV at 90-100mA. Right now,
                                I'm using a Fein Focus Tiger 160 for x-ray inspection of some copper
                                cored assemblies that we're building because I have to, that's the only
                                way we can inspect the BGA's. The copper core in the PCB won't allow
                                x-ray of the BGA's unless you use a system that can penetrate the core.

                                But if these devices can be damaged at such a low voltage (if indeed
                                Daniel's figures are correct), shouldn't Altera issue some sort of
                                warning to their customers about x-ray damaging the devices? After all,
                                there will be a lot of customers using x-ray for inspection.

                                Kind regards,

                                -Steve Gregory-
                                Senior Process Engineer
                                LaBarge Incorporated
                                Tulsa, Oklahoma
                                (918) 459-2285
                                (918) 459-2350 FAX
                                __________________________________________________________________
                                This message may contain information that is privileged and confidential
                                to LaBarge, Inc.  It is for use only by the individual or entity named
                                above.
                                If you are not the intended recipient, you may not copy, use or deliver
                                this message to anyone.  In such event, you should destroy the message
                                and kindly notify the sender by reply e-mail.

                                ---------------------------------------------------
                                Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
                                unsubscribe, send a message to [log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
                                (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
                                Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
                                posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
                                archives of previous posts at: http://listserv.ipc.org/archives Please
                                visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
                                additional information, or contact Keach Sasamori at [log in to unmask] or
                                847-615-7100 ext.2815
                                -----------------------------------------------------

                                ---------------------------------------------------
                                Technet Mail List provided as a service by IPC using LISTSERV 1.8e
                                To unsubscribe, send a message to [log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF Technet
                                To temporarily halt or (re-start) delivery of Technet send e-mail to
                                [log in to unmask]: SET Technet NOMAIL or (MAIL)
                                To receive ONE mailing per day of all the posts: send e-mail to
                                [log in to unmask]: SET Technet Digest
                                Search the archives of previous posts at: http://listserv.ipc.org/archives
                                Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
                                for additional information, or contact Keach Sasamori at [log in to unmask] or
                                847-615-7100 ext.2815
                                -----------------------------------------------------

                                ---------------------------------------------------
                                Technet Mail List provided as a service by IPC using LISTSERV 1.8e
                                To unsubscribe, send a message to [log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF Technet
                                To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
                                To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
                                Search the archives of previous posts at: http://listserv.ipc.org/archives
                                Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
                                -----------------------------------------------------



                                __________________________________________________________________
                                This message may contain information that is privileged and confidential to LaBarge, Inc.  It is for use only by the individual or entity named above.  If you are not the intended recipient, you may not copy, use or deliver this message to anyone.  In such event, you should destroy the message and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2