Hi Inge!
You sent me this picture some time ago, along with one of your beautiful SEM
images and the EDAX chart of it, remember?
http://stevezeva.homestead.com/files/bga002.jpg
http://stevezeva.homestead.com/files/BGA_SEM.jpg
http://stevezeva.homestead.com/files/BGA_EDAX.jpg
Steve
--------------------------------------------------
From: "Inge" <[log in to unmask]>
Sent: Wednesday, April 21, 2010 4:26 PM
To: <[log in to unmask]>
Subject: [TN] BGA balls dipped in sugar?
> Hi,
> at least it looks so. It's ordinary lead tin soldering process. Analysis
> gave that what looked like sugar crystals probably was Lead Carbonate.
> How is that created? If someone got same, what did you do then? You need
> extraordinary stuff to remove these crystals.
> Sent picture to Steve.
> /Inge
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|