DI Water itself is not corrosive, but it is aggressive, if you get the
difference. Having been stripped of all it's ionic content, it's "hungry"
to replace those ions, and will draw them from wherever it can. That's what
makes it so effective at removing ionic contamination from boards. However,
it doesn't discriminate about where it draws ions from, and draws them just
as readily from seals and gaskets if it can. Domestic appliance seals are
not resistant to this sort of attack, and the loss of ionic content from
their composition degrades them to the point where they fall apart and dump
more dirt back onto boards than is ever removed. The machines then leak and
eventually become useless for anything.
Peter
Rudy Sedlak <[log in to unmask]> 10/07/2002 09:08 PM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to RSedlak
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: Re: [TN] Water soluble batch washers.../deionized water
The "hazards" of deionized water are somewhat blown out of proportion.
Deionized water is not really that corrosive, only marginally more than tap
water...
HOWEVER, deionized water lacks the buffering capacity of tap water. (All
that water hardness serves to buffer the pH nicely) So, if the "stuff"
you are rinsing is corrosive inherently, the deionized water also becomes
corrosive, especially to metals.
However, most of the aqueous cleaners are pretty mild and non-corrosive, so
rinsing them with deionized water should be safe, even for the common home
dishwasher.
This is assuming that the ratio of (acidic/corrosive) flux on the parts in
the washer to the amount of alkaline cleaner being used is not so bad that
the wash water becomes acidic...then you have BIG problem.
The answer is to clean just a few boards, OR use a lot of cleaner to keep
the pH above 9, and preferably higher than that...
Rudy Sedlak
RD Chemical Company
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|