TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sat, 5 Jul 2008 17:39:03 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=UTF-8; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
And you mention only TC: the coefficient of hygroscopic expansion at 
constant temperature between, say, 25% and 75% RH (allowing time for 
stabilisation) is likely to be as much again per %RH.

Just the copper has a TCE of 16.6 µm/m/°C and that's inorganic. Organic 
materials have other molecular characteristics which render them 
mechanically unstable and not always predictable.

Brian

Werner Engelmaier /* wrote:
> Wow Jan,
> You have: "PCBs approx 450mm long, 50mm wide, 1.7mm thick, 12 layers, 17u 
> copper inner
> layers, Isola IS420 material, boards are produced with longest dimension in 
> warp direction in PCB production panel" �and you expect a 75um tolerance after 
> subjecting the PCB to board drying and leadfree reflow.
> 
> Just consider that in PCBs you are marrying 4 different materials [laminate, 
> prepreg, woven glass-fiber reinforcement, copper] together all of whom have 
> significantly different physical properties, particularly at different T's and 
> in different directions.
> 
> The laminate (which is fully cured) and the prepreg (not fully cured) have 
> different resin contents, go through glass transition (which changes molecular 
> structure and is not fully reversible, only nearly so), start to decompose at 
> SAC solder T's (actual weight loss, which is irreversible).
> 
> The glass-cloths is in your PCBs laid up with the warp direction in the 
> longest dimension in the PCB production panel making your PCBs quite non-uniform in 
> the x and y directions [the normal practice is to alternate warp and fill 
> directions on alternate layers to equalize the different properties in the warp 
> and fill directions�even with that, it is not uncommon to measure CTE-values 
> different in x and y by as much as 2 ppm/C].
> 
> The copper layers are mostly etched   away in irregular [in the sense of 
> physical behavior] patterns.
> 
> �and you expect a 75um tolerance after subjecting the PCB to board drying and 
> leadfree reflow?!
> 
> 
> 
> Werner
> Future workshops:
> Pb-Free Soldering Processes�Survival, Quality, Reliability, July 17/18, Thal, 
> Switzerland
> Pb-Free Soldering Processes�Survival, Quality, Reliability, July 21/22, Bad 
> Segeberg, Germany
> Pb-Free Soldering Processes�Survival, Quality, Reliability, August 18, O
> rlando
> Reliability Issues with Lead-Free Soldering Processes, September 22, 
> Schaumburg
> Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, 
> ENIG), September 22, Schaumburg
> Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia
> Solder Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania
> Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia
> 
> 
> 
> **************
> Gas prices getting you down? Search AOL Autos for 
> fuel-efficient used cars.
>       (http://autos.aol.com/used?ncid=aolaut00050000000007)
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2