What's wrong with this picture? Low cost - over 280 Tg - that bow and twist?
Polyimide tops out at 270 and shouldn't be cured over 250. CLTE and Rogers
counterpart, as 4003, tops out at 280. Pure ceramic is your very expensive,
impossible answer for now and ever more.
Building a space shuttle are we?