TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Charles Barker <[log in to unmask]>
Date:
Tue, 4 Nov 1997 10:11:03 -0600
Content-type:
text/plain; charset=US-ASCII
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (52 lines)
Charles Barker@IO-US
11/04/97 10:11 AM

Graham,

We are using water soluble spacers from BIVAR. I believe they are available
in different thicknesses.

Regards,

Charlie B.




Please respond to [log in to unmask]; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Charles Barker/IO-US)
Subject:  [TN] Mechanical standoff




Good Day Technet!
In wavesolder attachment of some through hole components, we have to
provide a temporary standoff to keep the part off the board surface.
Currently we are doing this with bits of wire or other mechanical means,
which are then removed after wavesolder.  Some components we keep off
the board with a washable solder masking material, but this is not a
precise or quick method.  Is there such a thing as a preformed standoff
that will dissolve when the assembly is washed, that would be put on the
lead before insertion into the board?
Thanks!
Graham Collins
Process Engineer,
Litton Systems Limited, Atlantic Division
(902) 873-2000 ext 215

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2