TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Mon, 19 Jun 2006 11:33:51 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Paul

If your environment approaches anything reasonable, you should not have a
problem. As part of the verification process we used, ImAg boards were held
for over a week between the two reflow process and still soldered very well.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389

----- Original Message -----
From: "Black, Paul" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, June 19, 2006 11:26 AM
Subject: [TN] ImAg Solderability


> Hi TechNetters,
>
> I have a double sided board that uses an ImAg finish. I run one side on
> one SMT line and the other side on a separate line, but sometimes the
> second line is being used for other product and may not be available for
> up to a week. I understand that ImAg tarnishes over time and have also
> heard that subjecting the board to reflow will speed up the tarnishing
> process on unsoldered pads. Should I be worried about solderability issues
> on the second side of my board if I wait a week in between processing the
> two sides? I am running a no-clean, leadfree process without nitrogen, and
> the boards reside in a 40% - 50%RH environment.
>
> Thank you,
> Paul Black
> Manufacturing Engineer
> Kronos
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2