TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Fri, 18 Mar 2005 10:37:58 -0500
Reply-To:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (80 lines)
if you put 1+2+3, it will freeze the last... ;-)

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brian Ellis
Sent: Friday, March 18, 2005 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] Friday question


It all depends what you mean by freezing. If you allow mushy ice
crystals, then sucrose, ethylene glycol, calcium chloride.

Brian

Precision Analytical Lab wrote:
> This one's real fun.  It's sure to make blood shoot out your nose.
>
> Which of these 3 solutions will freeze first, second, and third and WHY
will
> they freeze in that order????
>
> 1) 10 grams of Calcium Chloride (road salt) dissolved in 20 mL of DI
water.
>
> 2) 10 grams of Sucrose (table sugar) dissolved in 20 mL of DI Water.
>
> 3) 10 grams of Ethylene Glycol (antifreeze) dissolved in 20 mL of DI
water.
>
>
> Shawn Parson
>
> Precision Analytical Laboratory
> 4106 Cartwright Drive
> Suite A
> Kokomo, IN  46902
> Ph: (765) 455-1993
>
> Specializing in Ion Chromatography (IC) and Surface Insulation Resistance
> (SIR)
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2