TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 29 May 1997 11:18:54 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13001
X-Sender:
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Fri May 30 07:
00:13 1997
X-Loop:
Resent-Message-ID:
<"dvSfg.0.qp2.WnPZp"@ipc>
Subject:
From:
Sheila Smith <[log in to unmask]>
>From bergdi Thu May 29 11:
47:13 1997
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wX8Ls-000BjPC; Thu, 29 May 97 11:47 CDT
X-Mailer:
Windows Eudora Pro Version 2.1.2
Message-Id:
Parts/Attachments:
text/plain (20 lines)
Maurice,

ASTM 2240 describes making Shore hardness measurements.  Shore durometers
are available from Pacific Transducer Corp, Los Angeles CA.  Alternately,
many mechanical test labs can do Shore hardness measurements.  Please email
me directly if you'd like more information.

Sheila Smith, Tracor  AES

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2